Nominal Composition

Weight %

Nickel: 56 Balance
Chromium: 22
Molybdenum: 13
Iron: 3
Cobalt: 2.5 max.
Tungsten: 3
Manganese: 0.5 max.
Silicon: 0.08 max.
Carbon: 0.01 max.
Vanadium:  0.35 max. 
Copper:  0.5 max. 